TENSILE CREEP TESTING MACHINE FNCT NCTL NOTCHED CREEP TESTER ISO 16770


Unit Price:

Not informed

FOB Price:

Not informed

Minimum Order Quantity:

Not informed

Type of Payment:

Not informed

Preferred Port:

Not informed

Reference:

Not informed


Description

Full Notch Creep Tester-2 NCT- Tensile Creep Tester
FNCT is widely used method to classify polyethylene materials in regarding to their slow crack growth behaviour under accelerated conditions.
Conforming to standards ISO 16770 and DVS 2203-4 ,
Number of stations as customer request,
10 inch touch display,
report as EXCEL file,
100l of tank capacity,
Temperature up to 95 C,
Load ranges as request,

  • FNCT
  • full notch creep
  • HDPE creep test
  • NCTL
  • 2NCT
  • constant load creep

Production Capacity:

Not informed

Delivery Timeframe:

Not informed

Incoterms:

Not informed

Packaging Details:

Not informed


More about
AHP PLASTİK MAKİNA

icone de usuario

10-50

Employees

sales icon

1M - 2M

Sales volume (USD)

icone de exportar

50%

% Export sales

2003

Year

Established


Business type
  • Industry / Manufacturer

Keywords
  • hydrostatic pressure test
  • DSC
  • OIT
  • oxidation induction time
  • carbon content tester
  • tensile tester
  • universal tensile
  • Ver Mais

Contact and location
  • icone de usuario Mohammad ********
  • icone de telefone +90 54********
  • map-marker Beylikduzu / Istanbul | Turkey

Make your Request!

Make your Request!

Start conversation
logo-Whatsapp

Hello 👋!
Can we help you?

Start conversation Start conversation

Fill in your full name and phone number 😁

Start conversation Start conversation